纳米晶高矩形比尖峰抑制器磁芯具有中低饱和磁感应(Co基非晶0.58T;Fe基纳米晶1.2T)、低矫顽力、低损耗、优异的耐磨性和耐腐蚀性、低对温度的依赖性


 咨询电话:+86-13316196042


产品详情


纳米晶高矩形比尖峰抑制器磁芯 Nanocrystalline High Rectangular Ratio Spike Suppressor Magnetic Cores

 

纳米晶高矩形比尖峰抑制器磁芯具有中低饱和磁感应强度(钴基非晶0.58T, 铁基纳米晶1.2T)。 低矫顽力, 低耗损, 出色的抗磨损和耐腐蚀能力,对温度依赖性低。具有非常高的矩形比,在很小的电流下就可以达到饱和,可用于漏电保护

Fe-based Nanocrystalline Co-based Amorphous High Rectangular Ratio Magnetic Cores possess a mid and low saturation magnetic induction(Co-based Amorphous 0.58TFe-based Nanocrystalline 1.2T), low coercivity, low loss, excellent wear and corrosion resistance, low dependence on temperature

 

经典应用 Typical Application:

磁放大器

Magnetic Amplifier(MagAmp)

 

漏电流互感器

Leakage Current Transformer

 

磁传感器

Magnetic Sensor

 

尖峰抑制器

Spike Suppressor

 

 

铁基纳米晶和钴基非晶高矩形比磁芯对比 Comparison of Fe-based Nanocrystalline Co-based Amorphous High Rectangular Ratio Magnetic Cores:

项目/Item

单位/Unit

钴基非晶参考值

Co-based Amorphous

Reference value

铁基纳米晶参考值

Fe-based Nanocrystalline

Reference value

饱和磁感应强度Saturation Flux Density(Bs)(25℃)

T

0.58

1.2

饱和磁致伸缩系数Saturation Magnetostrictive Coefficient (λs)

-

0.2x10-6

 

双级磁通密度Bipolar Flux Density(25℃)

T

1.15

2.38

双级磁通密度Bipolar Flux Density (90℃)

T

1

2.07

矩形比Rectangular Ratio Br/Bs

-

96%

92%

居里温度Curie Temperature

400

570

连续工作温度Continuous Operation Temperature

90

120

 

铁基纳米晶和钴基非晶高矩形比磁芯曲线对比 Curves Comparison of Fe-based Nanocrystalline Co-based Amorphous High Rectangular Ratio Magnetic Cores:

 

图1 钴基非晶及铁基纳米晶高矩形比磁滞曲线

Fig.1 Hysteresis Loops of Co-based Amorphous and

Fe-based Nanocrystalline High Rectangular Ratio

图2 铁基纳米晶损耗曲线

Fig.2 The Core Loss Curve of Fe-based Nanocrystalline

图3 钴基非晶损耗曲线

Fig.3 The Core Loss Curve of Co-based Amorphous

 

铁基纳米晶高矩形比磁芯规格 Fe-based Nanocrystalline Product Specification

金磁海纳料号P/N

磁芯尺寸

Core Dimensions

成品尺寸Finished Dimensions

有效截面积

Core Cross-section  

有效磁路长度

Mean Core Path Length

磁芯重量

Core Mass

OD(mm)

ID(mm)

HT(mm)

Ae (mm2)

Le(cm)

m (g)

JCMA-1303-W01

12.8x9.5x3.2

14.7

7.9

4.8

0.042

3.5

1.1

JCMA-1205-B01

12x8x4.5

14

6.6

6.2

0.07

3.14

1.7

JCMA-1205B-W01

12.5x10x5

14

8.5

6.8

0.05

3.53

1.4

JCMA-1505-W01

15x10x4.5

17.1

7.9

6.5

0.09

3.93

2.7

JCMA-1606-W01

16x10x6

17.9

8.2

8.2

0.144

4.08

4.5

JCMA-1806-W01

17.5x12.5x6

19.1

10.9

8.1

0.12

4.71

4.4

JCMA-1905-W01

19x15x5

21.2

13

7.3

0.08

5.34

3.3

JCMA-2008-W01

20x12.5x8

22.6

10.3

10.2

0.24

5.1

9.4

JCMA-2510B-W01

25x20x10

27.7

17.1

12.9

0.2

7.1

10.9

备注:可以根据客户要求定制Other customized designs are available according to client's requires

 

钴基非晶高矩形比磁芯规格 Co-based Amorphous Product Specification

金磁海纳料号P/N

磁芯尺寸

Core Dimension

有效截面积

Cross section
area

有效磁路长度Magnetic
Iron Path
Length

 

 

重量Weight

 

 

裸磁芯尺寸

Bare Core Dimension
ODxIDxH(mm)

成品磁芯尺寸

Finished Core Dimension

OD(mm)
(max)

ID(mm)
(min)

H(mm)
(max)

Ae
(cm2)

Le
(cm)

m
(g)

JCMA-1204-H

12x8x4

14.1

5.9

6.1

0.064

3.14

1.53

JCMA-1305-H

12.5x10x5

14.6

7.9

7.1

0.05

3.5

1.34

JCMA-1303-H

12.8x9.5x3.2

14.9

7.4

5.5

0.042

3.5

1.12

JCMA-1505-H

15x10x4.5

17.1

7.9

6.6

0.09

3.92

2.68

JCMA-1606-H

16x10x6

18.1

7.9

8.1

0.144

4.01

4.47

JCMA-1806-H

17.5x12.5x6

19.6

10.4

8.1

0.12

4.67

4.3

JCMA-1905-H

19x15x5

21.1

12.9

7.1

0.08

5.34

3.25

JCMA-1910-H

19x15x10

21.1

12.9

12.1

0.16

5.34

6.49

JCMA-1905-H

19x17x5

21.1

12.9

7.1

0.044

5.64

1.72

JCMA-2008-H

20x12.5x8

22.1

10.4

10.1

0.24

5.1

9.31

JCMA-2510-H

25x20x10

27.1

17.9

12.1

0.2

7.03

10.74

JCMA-2505-H

25x23x5

27.1

20.9

7.1

0.04

7.54

2.29

JCMA-2507-H

25x20x6.5

26.5

19.3

7.3

0.138

7.06

7.42

 备注: 可以根据客户要求定制 Other customized designs are available according to client's requires


关键字:

尖峰抑制器磁芯


感谢你对金磁海纳材料的关注

请将您的业务需求发送给我们、 我们有专业的服务团队来回答你!

相关产品

探索更多产品 >

Copyright 2023 广州金磁海纳新材料科技有限公司